What is the thickness of the national standard FRP ventilation duct?
Plate thickness of organic glass fiber reinforced plastic air duct in medium and low pressure system (mm)
Diameter d of circular duct or length b of rectangular duct.
wall thickness
D(b)≤200
2.5
2003.2
400D4.0
630D4.8
1000D6.2
Table 4.2.2-4 Thickness of Inorganic FRP Pipe for Medium and Low Pressure System (mm)
Diameter d of circular duct or length b of rectangular duct.
wall thickness
D(b)≤300
2.5~3.5
3003.5~4.5
5004.5~5.5
10005.5~6.5
15006.5~7.5
D(b)>2000
7.5~8.5
- Previous article:The prescription Jianling decoction is named as
- Next article:Will rural commercial banks fail?
- Related articles
- How is domestic violence graded?
- Who can give me some tabloid content about the 61st anniversary of National Day?
- Toxic and side effects of herbs
- What do people eat at the Cold Food Festival?
- What are the influences of traditional culture?
- Recognition and Understanding of Cloud Gaming
- Knowledge and Understanding of China's National Defense Construction
- Financial control model has several kinds of
- What are the similarities and differences between financial enterprise accounting and industrial enterprise accounting methods?
- Athletic pants wear well